Combine equal parts of our pine tar and purified organic linseed oil.
Spray a paint primer over the wood.
Wirebrushed 1 side smooth 1 side.
Western red cedar weathered silver grey pine v groove 1 side 2 x6 actual.
Green will soon be available too.
Pine tar is for exterior applications and creates a stain like finish.
It also takes down the stickiness of the surface so that it is more pleasant to touch or walk on.
Above grade we recommend mixing the pine tar 50 50 with allback purified raw linseed oil and applying warm so that the pine tar and oil mixture really penetrates the wood.
Ideal for barns and outbuildings wide plank siding decks porches fences fence posts etc.
Plywood siding t1 11 48 00 in.
Impregnate and reinforce wood to resist moisture and microbes while still allowing the wood to breathe and to keep it from drying out and cracking.
Black brown and red.
Use this organic raw linseed oil produced at our.
Pine tar is a natural wood preservative from the forest obtained by slowly burning the resin from the root stock of pine trees.
Wood siding shake wood siding 4 inch siding 1 in.
This mixture offers the best of both preservation and nourishment for the wood.
Pine tar also known as pitch is a great preservative of wood it s been used for centuries on wooden boats to prevent leaking and rot.
Let the primer dry for 30 60 minutes before painting the pine object.
It is available in a light and a dark finish as well as pigmented.
In this state pine tar has the consistency of molasses and can be used for preserving wood even below grade.
Heat to 80 degrees f and mix thoroughly.